Barium Titanate Ceramics

Barium titanate batio3 ceramics have been fabricated using powders prepared by sol-gel, coprecipitation and mixed oxide methods.The powders prepared by sol-gel and coprecipitation have average crystallite diameters of 100 nm and 300 nm, respectively while the diameter of the mixed oxide powder is 13 m.When sintered at the same temperature of 1320c, the three batio3 ceramics.